So I need to process some 4x5 TMax 100 I shot today and realized that I'm out of my usual developer, TMax RS. I have some D76 here that I guess I can try but I've yet to use this developer. Is there anything I should know before I begin?
I usually process starting with the times on the Massive Dev Chart. In this case is recommends 1+1 for 11:15 at 20 degrees Celsius or stock strength for 5:45. Is there a benefit for either way?
Also, I usually agitate for the first minute and the for 10 seconds every minute following. Same process for D76?
Anything else I should keep in mind?
Thanks in advance!
Tim
www.ScottPhoto.co
Bookmarks