Hi,
I've been using the Tetenal kit for two weeks now, and I've noticed some uneven development here and there, but usually fixable.
Yesterday I got one that was really bad, and I'd like to try and figure out what's going on before processing more film.
I use a Jobo 2553, two reels, twelve sheets of film, on a motorized base.
Pre-soak is at 40˚C (102˚F) for one minute, and I fill the tank completely with water.
Development is 3:30 at 40˚C, and Blix is 6:30 at the same temperature.
I wash for five minutes, emptying the tank at least seven times, then add stabilizer (to which some PhotoFlo has been added) for a minute, and hang to dry.
Most of the film comes out looking good with no issues.
Here's what I got yesterday:
Any thoughts or ideas as to why this is happening would be greatly appreciated.
Thanks in advance.