I use predominantly Fuji Provia, but also use other Fuji E6 and find that the processing times are different. Fuji Provia needs a First Developer time of 7 minutes while other Fuji E6 I have tried needs 7 1/2 Minutes.
Kodak E6 that I have processed requires only 6 minutes.
My biggest problem is with the Blixing stage. I am Blixing for 6 1/2 minutes (I have increased this from the standard 6 minutes) but still find that the films are coming out slightly fogged. If I dry them and then drop them back in the blixing solution for 10-15 seconds and then rinse and dry again the prints are perfect... Has anyone had any similar problems?