I did a batch of tri-x yesterday in xtol 1:3 and a good chunk of the negatives with a lot of smooth sky ended up with less density on the sky edge in the negative. I processed at about 70 degrees for 12 minutes. Aside from the strange edges the negs look pretty good. I've never had that trouble using hc110 for 9 minutes in the jobo 3010. Could that added development time had something to with it? Thanks.