Originally Posted by
Todd
Yes I agree, obviously something changed.
The premise is that the blotching is caused by the film touching during dev and therefore the chemicals not getting to that area. This is confirmed by the reduction to 4 sheets as they are physically more separated.
So to me this rules out chemicals. (I use the kodak single use chem kit).
What has changed is
--the re-introduction of Velvia 50
--I have added Provia
--I moved to a much more humid climate
My first suspicion is that the acetate based changed on the Fuji films and is now more flimsy causing the film to flex during the rotation and then stick together.
Of course this is pure speculation, I don't have any specs on this.