This is going to take longer than I thought, life gets in the way. Here's a partial list of film developers, I haven't gone thru all of the books yet:

Burki's Pyro

Standard Glycin

SD-19 Hot Shot

DeFero's DK-20X

Sease #3 Fine Grain

Edwal #12

Defender ND-3

777 Fine grain

Defender D-6

King's All-in-One

D-1 pyro

D-7 pyro

D-8 caustic

D-11 M-Q

DK-15 tropical

D-19 high

DK-20 M-Q

D-23 soft

D-25 fine

D-32 warm-tone

DK-50 M-Q

DK-60a M-Q

D-61 M-Q

D-72 M-Q

D-76 M-Q

D-82 extreme

D-84 pyro

D-85 lith

DK-93

Agfa17 borax

Agfa17M metaborate

Agfa20 M-Q

Agfa22 M-Q

Agfa30 X-ray

Agfa40M-Q

Agfa42 M-Q

Agfa45 Pyro

Agfa47 M-Q

Agfa48M metaborate

Agfa61 M-Q

Agfa64 tropical

Agfa70 caustic

Agfa72 glycin

Agfa73 extreme

Agfa79 lith

Agfa81 lith

Agfa90 high

Ansco 12 Fine grain

It looks like there are even more formulas for paper , toners, misc. I think this will be an on-going project.