Originally Posted by
Andrew O'Neill
I prefer to use a ziplock bag with developer poured inside. The bag combo is placed in a flat bottom tray. Puff a bit of air inside the bag, seal, and Bob's yer uncle. You won't need as much solution as you would with the hanger/tank method.
I'm currently working on some xray green latitude film and pyrocat-hd curves using 1+1+200 and 1+1+100 dilution. I also have curves for Rodinol. works very well with this developer. A few months ago I generated some reciprocity data that has been serving me well. I do believe I posted it here somewhere.