How did you matin temp during the process. Did you set the tray in some warm water or did it hold the temp enough to get through the processing times?
I just used the SP-810 and was so impressed. Its always a pain to try to develop my 4x10's and this worked perfectly. Well almost. I forgot to remove the little holder/spacers for 4x5 5x7 from the lid and managed to rub a couple holes in my first batch of negs. But I removed the holders and the rest of the negs turned out perfectly.