Thodoris, thanks - I have processed several dozen 8X10 sheets in trays. Managed to finally have some luck with minimal scratching while processing 4 sheets at a time, but was not satisfied with any scratches, so tried processing in 1 ltr upright tanks - 2 film hangers at a time, but got very uneven development no mater what I did - more rigorous agitation, less rigorous agitation - just could not make it work. Tried one film hanger laying flat in a tray but still got some processing streaks. I tried processing in an 8X10 Colourtronic daylight processing tube that I purchased many, many years ago when I was printing color slides via Cibachrome. The tube is 4 inches inside diameter and has small raised ribs that run the length. The ribs left marks on the X-ray film during processing
Anyway, the search continues.