I bought some of this (RC luster), loaded it, shot it, developed it and got 4 nice clean white sheets of expensive wet paper... I've never used positive paper before and wasn't sure which side was the emulsion, so loaded them how I thought it went.
Since this is positive paper, does white after dev-fix-wash mean that I totally super-over-exposed all 4 sheets a la light leak, OR does it mean that I loaded the paper backwards, and shot the base? I'm thinking the former. But my capacity for error is legion, so I'm open to other idiotic things I might have done.