Thanks for that- not sure the Tetenal stuff is quite what I need though - gold ammonium thiocyanate. I'm still very new to all this so I may of course be entirely wrong!
Meanwhile, here are a couple more successful efforts with Argyrotype from me. As before, both 8x10 contact prints on 11x14 Bergger Cot 320 paper in Lotus printing frame; Chamonix 810V and Nikkor-SW 150 f/8 (FP4+ processed in Pyrocat HD / BTZS Tubes)
and
So far all exposed with sunlight. I'll try to get a lamp setup soon to get some more done. Work getting in the way somewhat...!