I have been using Maco 820c and have figured out processing. I liked the film because I could shoot it in 120 or 4X5.
Now I have Rollei 400IR. I shot 6 sheets. I could not find any help for development times however so I did the following:
XTOL 1 to 2 for 14 min at 68 degrees F. with continuous agitation.
All but 2 of the six negatives came out hopelessly thin.
Has anyone figured a good way to develop this in XTOL?