Originally Posted by
Alan9940
I have a CPP-2 and have processed LF film in Expert Drums for many years using Pyrocat-HD at 1:1:100 and at 2:2:100 (for alt process.) IMO, running the drum at speed 4 is too fast for any staining developer due to possible oxidation. I spin the drum using the slowest speed possible and never had any issues. Best to do your own testing to arrive at proper development times for your chosen film(s). As a starting point, use times from the Massive Dev Chart and reduce by about 15%.