I'm new to 8x10 and realizing it is indeed a completely different game, even compare to 4x5!
Am I right to conclude this is caused by initial developer contact with the emulsion?
- I don't have the lift on my JOBO processor, and I'm using the print drum with the cup lid to develop films. There is a short time frame when the developer is poured inside the drum before I place it on the rollers and turn the processor on. Which would explain why the streak is on the long side.
(FOMA100, Rodinal 1+45, 9 min at 20C)
Or would you suggest some other causes? Thanks for your time guys.