This is my first post. Im new to LF and Im having trouble with tri-x320. I am using a unicolor drum and motor base. Im using about a liter/34 oz of D76 1:1, Fix, and Hypo clear. What I am seeing is my film still looks a little pink. Im fixing for approx 10 mins and hypo for 2 mins. I tried this same process with Tmax 400 with now issues. My develop time is 9 min @68 degrees F. I do a 10 min wash in the drum at the end allowing the water to fill the drum and constantly run. I empty the water about 4 times during this process.
My question is does tri x stay a little pink or should it be completely clear? Am I missing something, or doing something wrong? If anyone has suggestions please chime in.

Greg