Originally Posted by
IanG
That sounds like a very short dev time for Xtol 1+3, you don't say what temperature. It's around 2/3rds the time I use with Xtol & Tmax100 full strength.
I notice that the Kodak datasheet I have doesn't give a time for 1+3. You also don't sat what volume of developer, too little at that dilution and it will rapidly be exhausted, again contributing to under development.
The pink colour is a dye incorporated in the emulsion and Tmax films need longer than normal fixing times to remove this.