Hey Guys & Gals,
I decided I'd make my prints for the print exchange with the Oriental Warm Tone paper. I've read so many good things about it, it seemed like the thing to do to share with other LF shooters. I made my 10 prints. Fixed them for 12 minutes. Washed them for 60 minutes (in a rotary drum continuous water exchange). When I squeegeed them for drying, I noticed most had yellow edges. A few had stains that were dark and appeared as exposure problems, but in the shape of chemical stains.
Anyone had a similar experience? And does anyone have a solution? My thought is that the yellow is from the hypo. Should they be re-fixed? (I put a drop of Hypo Check in the hypo a number of times, and it came out good.) Questions, questions, questions.