Originally Posted by
Andre_941
Why are Pyro Negativess Delicate, and What to Do About It?
I noticed that both my sheet film and roll film pyrocat HD negs (water stop, TF-4 fix) are easily suseptible to physical damage. The 'easily scratched' part I understand as there is no hardener in the process per se. But what I don't get are the tiny (and not so) approximately circular flakes of missing emulsion on random areas of post-processed pyro negs.
Anyone else notice this tendency? Any solutions? Does anyone has a formula/product to recommend for hardening pyrocat negatives?