Here is the email trail
On 2019-02-22 12:45, steve@kronuswarp.com wrote:
> Bud,
> I determined the problem. It is the HP5-400. For some reason, it
> does not like semi-stand processing for an hour. I ran two sheets of
> Acros 100 for semi-stand development at 1 hour and it worked just
> fine. Only 1 or 2 pinholes at the most. I will try with Tmax100 next
> and hopefully it works out fine as well.
>
> So, it was not the PyrocatHD, but the HP5-400.
>
> Steven Ruttenberg
> PHOTOGRAPHER/ENGINEER
> Sgt/USMC 1983-1991
> _HTTP://WWW.STEVERUTTENBERGPHOTOGRAPHY.COM [1]_
> steve@kronuswarp.com
>>
> Links:
> ------
> [1] http://www.steveruttenbergphotography.com
steven;
We found that the Pheidone that we had recently purchased also had
problems. After mixing,or looked like it had been mixed well, it would
not stay in solution. The residue may have helped with the pin holes.
Since we have tried to recall all of the Pyrocat HD kits. By recalling
we are replacing those kits and please do not return unused portions.
But please let us know the particulars of your order and we will wend
oiut a new one.
The problematic Phenidone came from Artcraft chemical, and we have been
able to replace