For processing multiple sheets of film I use a
JOBO 3010 (4x5)
JOBO 3005 (Full Plate and 8x10)
JOBO 3062 (11x14, yes I know it was made to be used with processing paper but have had no edge density problems with it when processing 2 11x14" sheets in the drum.
JOBO publishes a range of chemical volumes:
JOBO 3010 210ml-330ml
JOBO 3005 330ml-630ml
JOBO 3062 no published info so I use the 3005's max of 630ml.
I have been using the maximum volumes with each of the tanks.
Developers: Diafine or Rodinal (with the occasional HC110 B).
Have the feeling that I am using too much chemistry and throwing too much developer down the drain.
Anyone out there successfully using less chemical volumes?
thanks