I looked, I really did, but I wasn't able to find the following specific information for developing sheet film in Pyrocat HD. If you know, please tell me or, if you would be so kind, point me to the URL for:

FP4+
HP5+
Acros
Delta 100
Tri-X

developing times in TRAY at 68 DEG for silver, Azo and also for Pt/Pd (90% Pd). So the chart below completed would be very helpful. I thank you expansively!


ISO/TIME


SILVER....................AZO.................... Pd/Pt

FP4+
HP5+
Acros
Delta 100
Tri-X

IanG
24-May-2011, 10:31
Can only give times for Silver but I process all those films (except Tri-X which I don't use) for 15 mins 1+1+100 @ 20°C (68°F). That's in a tray or a tank.

Ian

mdm
24-May-2011, 10:39
http://unblinkingeye.com/Articles/PCat/PCat4/pcat4.html

Tony Evans
24-May-2011, 10:46
Also some info at
http://unblinkingeye.com/Articles/Pyrocat/pyrocat.html

chris_4622
24-May-2011, 11:03
I use Fp4+ for printing on Lodima grade 3. Pyrocat Hd 2:2:100 in tubes for 9 minutes is my normal time.

chris

Scott Davis
25-May-2011, 06:46
I do Pyrocat HD 1:1:100 in a Jobo Expert drum for FP4+ for 13 minutes @ 75F for Pt/Pd printing. Expose at ISO 64.

Marek Warunkiewicz
25-May-2011, 08:04
Richard, look here, some of them are listed.

http://www.digitaltruth.com/devchart.php?Film=&Developer=Pyrocat&mdc=Search

marek