PDA

View Full Version : Ferrotype Release Agent



Barrie Smith
29-Dec-2000, 19:12
Hello!

Many years ago, before RC papers, commercially produced prints were dried on sma ll, or large, rotating, heated, polished drums for glossy finish.

I know that many workers still use these drums, or ferrotyping plats.

After the prints were washed, and just before they were placed on the drum, they were immersed in a solution called "ferrotype release agent", or "glossing agen t". This agent produced a higher gloss than would be obtained with water alone, and also helped prevent the prints from sticking to the drum.

A search of Kodak's web site, and others, has produced no agent suitable for thi s purpose.

I believe the primary ingredient was glycerin, but I'm not sure.

Does anyone have a source for this agent, or know how to make it?

Thank you, Barrie Smith, Missoula, Montana

Joseph Wasko
29-Dec-2000, 19:22
The trade name used to be Pakosol (circa 1971). I don't know if they are still around. There was also a ferrotype polish. Cleaning the ferrotype plates removes any residual emulsion. Stuck on emulsion can cause a gummy plate. Hope this helps.

Wayne_6692
29-Dec-2000, 19:54
Bon Ami was used to polish the plates.

William Leviit
2-Jan-2001, 09:25
A quick dunk in a wetting agent will also work. Tetenal makes a product called M irosol (I think) and it is specifically made to produce the best results when ferrotyping.

Charlie Stracl
2-Jan-2001, 13:58
I think Kodak's was Print Flattening Solution. If you check out darkroom books from the 50's & 60's glycerin was indeed recommended. These books would give you an idea as to the dilution to use.

david clark
6-Jan-2001, 23:55
Hi Barrie, I think you're right, it's glycerin, and some photoflo, and mostly water. I can't get to my records right now to find the right amounts of each, but I know it isn't critical. Basically I think you are slowing and evening out the drying process. Maybe that guy in Phototechnics who answers the chemical questions could give you the right amounts. But those were the ingredents I used last year. Good luck, David