PDA

View Full Version : Developing T-Max 100 with D-23



Delfino L. Tiongco
4-Feb-2000, 23:52
I need some data on using D-23 (one bath/two bath) process with T-Max 100. Any temperature/time info will be appreciated.

Delfino

Joseph Dickerson
10-Feb-2000, 15:59
This is not the answer you're seeking but rather my opinion on the matter. There is no advantage to using D-23 with T-Max films. They seem to respond much better to a non-Metol based formula. I use either T-Max RS developer or Agfa Rodinol.

The T-Max films are already fine grained without all the Sodium Sulfite of the D-23 formula and you will lose sharpness with D-23 as compared to either of the above mentioned developers.

If you choose to go with T-Max developer be sure to use the RS version. The original T-Max developer should not be used with sheet film.

William Marderness
10-Feb-2000, 18:57
I have tried D-23 1:1 with HP-5+ with interesting results. Compared to D-76 1:1, the contrast from Zone 1 through 5 is higher, and the contrast from zone 5 and up is lower. This provides high shadow contrast and low highlight contrast (a shoulder). My EI is 125 for N development.

With T-Max films, I think you will get a similar curve. I saw in a book (I don't remember which) that Microdol-X produced this type of curve with T-Max films. Microdol-X is D-23 (or similar to it) with the addition of 30g table salt.

Try the published times for D-76 and expect a low EI, 50 or lower.

William Marderness
10-Feb-2000, 19:02
One more thought, I suggest you dilute D-23 1:3, since T-grain films don't like high concentrations of sodium sulfite.