Robert Musgjerd
25-Aug-2004, 17:07
Has anyone out there been using classic 200 or 400 for pt and pd printing If so what have you been using as a developer and what speed have you shooting the film at thanks
sanking
25-Aug-2004, 18:44
Yes, Pyrocat-HD 2:2:100, rotary processing in tubes or Jobo with slow rotation at 72º F.
Scenes of normal contrast, JandC Classic 400.
DR 1.40 for 25:75 pt./pd. mix, 9 minutes.
DR 1.8 for straight palladium printing, 15 minutes.
Same times for JandC Classic 200.