I have recently made the jump from shooting 4x5 (TMax100 with D76) to 11x14 (Ber gger BPF200 with PMK) with a whole lotta learning curve and fun with some frustr ation in the process!!
In some of my prints (AZO+ Amidol), I have noticed a (negative) density increase along the edges - very difficult to even notice on the negative but very ugly o n the print. I develop one sheet at a time in trays, the trays are about 14"x18" .
I assume that this density is from uneven development due to the more vigerous m ovement of the developer over the edges of the film. Before I go out and buy a 18x22 tray (I never had the problem with 4x5 in 5x7 trays), I would appreciate v alidation (or not), of my theory and/or any other solutions/suggestions because this simply cannot continue!
Thanks for all the help!!