Heya,
So I'm processing FP4+ in PMK in a slosher and am getting blotchy skies.
Everything is at 70 degrees.
2' water bath
7'30" in PMK. Agitation is done by lifting one side of the tray twice (within 5 seconds) every 15 seconds i.e. top raised twice at 12, left raised twice at 9, etc.
45" seconds in water bath.
5' in fixer.
2' in PMK- agitation is every 30 sec done by pulling slosher out of PMK and then inserting it again.
20' wash in gravity washer.
I've only used PMK with efke before and haven't gotten stuff like this. Any thoughts?
Thanks
T.
Image is attached.