Hi, I just developed six sheets of T-Max 100 in a Jobo CPE 2, with the six sheet reel. Don't know the name or number...
This is the reel:
Anyway, I used X-Tol 1:1 at 20 degrees for 8m:45s, citric acid with water as stop bath for about a minute and 1+4 tetenal superfix plus as fixer for about four minutes.
Nothing much differnent as the last time, which is half a year ago (and another year the time before... ).
The first two slides came out perfectly fine, the next two seemed a bid cloudy to me, but when I saw the last ones, I know there is something off.
Here the slides in the same order:
to be continued in the next post...