  1. #41

    Join Date
    Oct 2013
    Location
    Doncaster UK
    Posts
    627

    Re: Fomapan 4x5 sheet film and Xtol

    I am developing my FomaPan 100 in Replenished Xtol for 6 minutes @20 °C but still feel I could do with reducing the dev time to control the highlights.

    Would going lower than 6 minutes create other issues.

  2. #42

    Re: Fomapan 4x5 sheet film and Xtol

    You ought to use a step wedge, develop at different times then use a densitometer. I don't shoot any emulsion until I've tested it. After that, I know exactly how I want it exposed & developed.

    Sent from my 0PJA2 using Tapatalk

Similar Threads

  1. FomaPan 100 4x5 Sheet Film & Kodak HC-110 Question
    By IanBarber in forum Darkroom: Film, Processing & Printing
    Replies: 17
    Last Post: 28-Oct-2016, 01:52
  2. Fomapan 100 failure, reciprocity and Xtol, minimal agitation
    By jumanji in forum Darkroom: Film, Processing & Printing
    Replies: 3
    Last Post: 1-Feb-2014, 10:56
  3. Fomapan 400 Sheet Film
    By Andrew O'Neill in forum Darkroom: Film, Processing & Printing
    Replies: 11
    Last Post: 7-Jul-2007, 19:37

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •